Mitigating stress corrosion cracking and irradiation defects in ods austenitic alloys by laser shock peening

Xueliang Yan, Yongfeng Lu, Michael Nastasi, Bai Cui

Research output: Contribution to journalConference article

Original languageEnglish (US)
Pages (from-to)1459
Number of pages1
JournalTransactions of the American Nuclear Society
Volume118
StatePublished - 2018
Event2018 Transactions of the American Nuclear Society, ANS 2018 and Embedded Topical Meeting Nuclear Fuels and Structural Materials - Philadelphia, United States
Duration: Jun 17 2018Jun 21 2018